A copper-nickel alloy of composition 60 wt% Ni-40 wt% Cu is…

Questions

A cоpper-nickel аllоy оf composition 60 wt% Ni-40 wt% Cu is slowly heаted from 1200°C (2192°F), whаt will be the composition of the last solid phase remaining just before the alloy completely melts?